Color fastnessCrockingGray Scale 1–5ISO 105-X12

Rubbing Fastness (Crocking)

How well color resists transferring when the fabric is rubbed, wet or dry
Color fastness property
Rubbing fastness, also called crocking, measures how much color rubs off a textile onto another surface when the fabric is rubbed. It is tested both dry and wet using a crockmeter that rubs a white test cloth against the specimen, and the staining of the white cloth is rated on the 1–5 gray scale — a key property for deep and surface-colored textiles.

A crockmeter rubs a standard white cotton cloth across the colored specimen under defined pressure and strokes, dry in one test and wet in another (wet crocking is almost always worse). The color transferred to the white cloth is rated on the gray scale from 5 (no transfer — best) to 1 (heavy transfer).

Rubbing fastness matters wherever color could mark skin, other garments or furnishings — dark denim, deeply dyed bedding, upholstery and especially pigment-printed or surface-colored fabrics, where color sits on the surface. Poor crocking is a common complaint (dark sheets marking mattresses, upholstery marking clothes). It depends on dye penetration, unfixed dye removal and, for pigments, binder quality; wet crocking is the harder hurdle and the one most often specified.

At a glance

TypeColor fastness property
What it testsColor transfer by rubbing (dry & wet)
StandardISO 105-X12 / AATCC 8
ScaleGray scale 1–5 (5 best)
Typical requirementDry ≈4, wet ≈3 and above
NoteWet crocking is usually the weakest

Characteristics

01Rates color rub-off (crocking)
02Tested dry and wet with a crockmeter
03Staining rated on gray scale 1–5
04Wet crocking usually worse than dry
05Critical for deep and surface colors

Typical uses

01Dark and deeply dyed bedding
02Denim and indigo textiles
03Pigment-printed fabrics
04Upholstery and contract textiles
05Any surface- or deep-colored product

Strengths

01Flags color that marks skin/surfaces
02Tests both dry and wet conditions
03Standardized 1–5 rating
04Guides binder and dye-penetration quality
05Prevents common staining complaints

Limitations

01Wet crocking hard for darks/pigments
02Surface colors inherently weaker
03Does not cover wash or light fastness
04Requires correct method and conditions
05One property among several

Where it applies

Rubbing (crocking) fastness is what stops a dark sheet marking a mattress, a cushion marking clothing or a printed fabric transferring color. It is rated dry and wet on the 1–5 gray scale, with wet crocking the harder, most-specified hurdle — typically dry around 4 and wet around 3 or above. It depends on good dye penetration, removal of unfixed dye and, for pigment prints, binder quality.

Home fashionHospitalityContractSustainable fashionFashion

Frequently asked questions

What is crocking?+
Crocking is the transfer of color from a textile onto another surface when it is rubbed. Rubbing fastness testing measures it with a crockmeter that rubs a white cloth against the fabric, then rates how much color transferred on the 1–5 gray scale.
Why is wet crocking usually worse than dry?+
Moisture mobilizes loosely held and surface color, so more transfers when the fabric is rubbed wet. Wet crocking is therefore the tougher test and the one buyers most often set a minimum for, especially on darks and pigment prints.
Why do dark sheets sometimes mark the mattress?+
Poor rubbing fastness — surface or unfixed dye rubs off under friction. It is addressed by better dye penetration, thorough removal of unfixed dye and, for pigment color, higher-quality binders and correct curing.

Sourcing with rubbing fastness (crocking)?

Vanvino® can source, specify and document textiles to your exact construction and quality requirements.

Request advice
Last updated · Published by Vanvino® · Editorial policy & corrections
Sources: AATCC · ISO