Specifying Textile Quality
The common mistakes are specifying one number in isolation ('40,000 rubs' with no method), mixing incompatible systems, or testing everything regardless of use. The fix is to match a handful of requirements to the real stresses the product faces.
Below are the comparisons that come up most, then a framework for building the specification. The individual test pages cover each method in full.
Martindale vs Wyzenbeek
Both rate abrasion resistance for upholstery, but they are different tests and their numbers do not convert. Martindale (ISO 12947) rubs in a multidirectional figure-of-eight and counts 'rubs'; it is the European reference. Wyzenbeek (ASTM D4157) rubs back-and-forth in a straight line and counts 'double rubs'; it is the US reference.
Specify the one your market uses — Martindale for European/global supply, Wyzenbeek for North America — and require both only if the product sells in both regions. Never convert between them.
Strength vs durability vs pilling
These measure different failure modes and a fabric can pass one and fail another. Strength tests (tensile, tear, seam slippage, bursting) ask 'will it break or pull apart under load?'. Abrasion (Martindale, Wyzenbeek) asks 'how long before the surface wears through?'. Pilling asks 'will it look worn (bobbled) even if it doesn't wear through?'.
A durable product usually needs a requirement from each relevant group — for example, for contract upholstery: abrasion (Martindale rubs), seam slippage, tensile strength, and pilling grade.
A framework for a sound specification
Work from the product's real life, not a checklist:
Frequently asked questions
Can I convert Martindale rubs to Wyzenbeek double rubs?+
Which tests should a contract upholstery spec include?+
Is a higher number always better?+