StabilityTested propertyShrinkageISO 5077
Dimensional Stability (Shrinkage)
How much a fabric changes size when washed or dried
Dimensional change (shrinkage)
Dimensional stability is a fabric's resistance to changing size — shrinking or, less often, stretching — when it is washed, dried or steamed. It is tested by marking a specimen, laundering it under a defined procedure, and measuring the change, reported as a percentage (a negative figure for shrinkage) in the length and width directions.
In the standard procedure, specimens are marked with reference points (ISO 3759), washed and dried under defined conditions (ISO 6330 or AATCC 135), then re-measured; the dimensional change is calculated per direction (ISO 5077). A result of −3% means the fabric shrank by 3% in that direction. Acceptance limits are typically a few percent, with tighter limits for fitted and sized products.
Shrinkage comes mainly from relaxation of tensions locked in during weaving, knitting and finishing, and (in wool) from felting. It is controlled in advance by mechanical pre-shrinking — sanforizing for wovens, compacting for knits — and by anti-shrink/anti-felt finishes. For bedding, fitted covers and apparel, dimensional stability decides whether a product keeps its size and fit after the customer's first washes, so it is a core acceptance test.
At a glance
PropertyDimensional change (shrinkage)
Measured inPercent change, per direction
ProcedureMark, launder, re-measure
Key standardsISO 5077, 6330, 3759; AATCC 135
Applies toWovens and knits
Controlled bySanforizing, compacting, anti-shrink finishes
Characteristics
01Size change after washing and drying
02Reported as % change per direction
03Negative figure means shrinkage
04Driven by relaxation of locked-in tension
05Controlled by pre-shrinking and finishes
Typical uses
01Bedding and fitted covers
02Sized and fitted apparel
03Tablecloths and made-up home textiles
04Acceptance testing against a % limit
05Validating sanforizing and compacting
Strengths
01Predicts real first-wash behavior
02Simple, comparable percentage figure
03Standardized across ISO and AATCC
04Protects fit and sizing
05Confirms pre-shrinking finishes work
Limitations
01Result depends on the wash/dry procedure
02Home laundering varies from the test
03Some residual change can remain
04Direction differences hide in a single value
05Procedure must be stated to compare
Where it applies
Dimensional stability is the test that decides whether bedding, fitted covers, tablecloths and sized apparel keep their size and fit after the customer's first washes — a frequent source of complaints and returns when it is ignored. It is reported as a percentage change per direction against an acceptance limit (often a few percent). Specify it with the laundering procedure named (ISO 5077/6330 or AATCC 135), and remember it is controlled upstream by sanforizing (wovens), compacting (knits) and anti-shrink finishes.
Home fashionHospitalityFashionContract
Frequently asked questions
What does a shrinkage result like −3% mean?+
It means the fabric shrank by 3% in that direction after the defined wash-and-dry procedure. Dimensional change is reported per direction (length and width); a negative number is shrinkage, a positive number is growth. Acceptance limits are usually a few percent.
How is shrinkage controlled?+
Mainly by mechanical pre-shrinking before the fabric is cut and sewn — sanforizing for wovens and compacting for knits — plus anti-shrink/anti-felt finishes for wool. These relax the tensions that would otherwise release as shrinkage in the first washes.
Why do my test and home-wash results differ?+
The test uses a defined, repeatable laundering procedure (ISO 6330 or AATCC 135). Real home washing varies in temperature, agitation and drying, so actual shrinkage can differ. The test gives a controlled, comparable figure rather than a guarantee for every wash.
Sourcing with dimensional stability (shrinkage)?
Vanvino® can source, specify and document textiles to your exact construction and quality requirements.
Request advice