StrengthTested propertyTear propagationISO / ASTM

Tear Strength

The force needed to propagate a tear once a fabric is nicked
Tearing (tear propagation) strength
Tear strength (tearing strength) is the force required to continue — propagate — a tear once a fabric has been cut or nicked, rather than the force to break it in tension. It matters because fabrics in use rarely fail by even pulling; they snag, nick and then rip. It is tested by the Elmendorf (ballistic pendulum) method or the tongue/trapezoid tear method, reported in newtons or grams-force per direction.

The Elmendorf test (ISO 13937-1 / ASTM D1424) uses a swinging pendulum to tear a pre-slit specimen in one rapid motion, giving the energy to propagate the tear. The tongue (ISO 13937-2) and trapezoid (ASTM D5587) methods pull a cut specimen on a tensile tester and record the tearing force. As with tensile strength, warp and weft are reported separately.

Tear strength is critical wherever fabrics are snagged or stressed at a point: bedding, upholstery, awnings, workwear, bags and outdoor textiles. A fabric can have high tensile strength yet poor tear strength (dense, tightly set fabrics sometimes tear easily because threads cannot shift to share the load). So tear and tensile are specified together, not interchangeably.

At a glance

PropertyTearing (tear propagation) strength
Measured inNewtons (N) or grams-force
DirectionsWarp and weft, reported separately
Key standardsISO 13937, ASTM D1424 (Elmendorf), D2261 (tongue)
Applies toWoven fabrics
MethodsElmendorf, tongue, trapezoid

Characteristics

01Force to propagate an existing tear
02Reflects real snag-and-rip failure
03Elmendorf (pendulum) or tongue/trapezoid (pull)
04Reported per direction (warp, weft)
05Not the same as tensile strength

Typical uses

01Upholstery, bedding and covers
02Awnings, outdoor and technical textiles
03Workwear, bags and heavy-use products
04Quality control against a target value
05Diagnosing fabrics that rip in service

Strengths

01Captures a common real-world failure mode
02Objective, comparable figure
03Standardized across ISO and ASTM
04Reveals warp/weft weakness
05Complements tensile strength

Limitations

01Only for wovens
02Elmendorf and tongue results differ
03High tensile does not guarantee high tear
04A single value hides direction differences
05Method must be stated to compare

Where it applies

Tear strength is the strength figure that reflects how fabrics actually fail — a snag that turns into a rip — so it belongs in any spec for upholstery, bedding, awnings, workwear, bags and outdoor textiles. Importantly, a high tensile strength does not guarantee good tear resistance; very dense fabrics can tear easily because the yarns cannot shift to share the load. Specify tear (ISO 13937 / ASTM D1424) alongside tensile, per direction and with the method named.

Home fashionHospitalityContractFashion

Frequently asked questions

What is the Elmendorf tear test?+
The Elmendorf test (ISO 13937-1 / ASTM D1424) uses a swinging pendulum to rip a pre-slit specimen in one motion, measuring the energy needed to propagate the tear. It is fast and widely used; tongue and trapezoid methods instead pull the specimen on a tensile tester.
Can a fabric be strong but tear easily?+
Yes. Tensile strength and tear strength are different failure modes. A very dense, tightly set fabric can have high tensile strength yet tear easily, because the yarns cannot move to share the load at the tear point. That is why both are specified.
Is tear strength reported per direction?+
Yes. Like tensile strength, tear strength is measured and reported separately for warp and weft, since the two directions usually differ in yarn and density.

Sourcing with tear strength?

Vanvino® can source, specify and document textiles to your exact construction and quality requirements.

Request advice
Last updated · Published by Vanvino® · Editorial policy & corrections